Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 870 MPa | 126000 psi | |
Arkema Group Orgalloy® RS 6000 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Tensile Creep Modulus, 1000 hours | 870 MPa | 126000 psi | |
Arkema Group Orgalloy® RS 6000CD Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Tensile Creep Modulus, 1000 hours | 870 MPa | 126000 psi | |
Arkema Group Orgalloy® RS 6000TLA Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |
|||
Tensile Creep Modulus, 1000 hours | 870 MPa | 126000 psi | |
Arkema Group Orgalloy® R 60ES Nylon 6 Alloy (Conditioned) Rigid polyamide 6 alloy: easy to process, low moisture absorption, chemical resistance (no known solvents). Blow extrusion grade for technical films: thermal resistance, barrier to gases and aromas,.. |