Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 500 - 850 MPa | 72500 - 123000 psi | Average value: 570 MPa Grade Count:5 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Tensile Creep Modulus, 1000 hours | <= 500 MPa | <= 72500 psi | DIN 53444 |
Zell-Metall Engineering Plastics Zellamid 1100 at 50% RH Zellamid® 1100 is the registered trademark for Zell-Metalls cast nylon 6 in different qualities.Our standard quality is a heavy duty, high impact, wear and heat resistant polyamide. It offers .. |
|||
Tensile Creep Modulus, 1000 hours | <= 500 MPa | <= 72500 psi | DIN 53444 |
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Tensile Creep Modulus, 1000 hours | 500 MPa | 72500 psi | ISO 899-1 |
DSM Stanyl® TE341 Nylon 46 (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 500 MPa | 72500 psi | ISO 899-1 |
DSM Stanyl® TW300 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 500 MPa | 72500 psi | ISO 899-1 |
DSM Stanyl® TW341 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 500 MPa | 72500 psi | ISO 899-1 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Creep Modulus, 1000 hours | 500 MPa | 72500 psi | ISO 899-1 |
BASF Ultraform® N2650 Z4 (LEV) POM Description: Is a POM + PUR, elastomer-modified injection-molding grades with high impact strength for clips, snap and fastening elements, also for components subject to impact stress.Information pr.. |
|||
Tensile Creep Modulus, 1000 hours | 500 MPa @Strain <=0.500 % |
72500 psi @Strain <=0.500 % |
ISO 899-1 |
BASF Ultraform® N2650 Z6 POM + PUR Description: Elastomer-modified injection molding grade for applications requiring highest impact strength together with low stiffness.Information provided by BASF |