Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 1800 MPa @Temperature 23.0 °C |
261000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Crastin® FG6129 NC010 PBT
(Unverified Data**) Crastin® FG6129 NC010 is an unreinforced, high viscosity polybutylene terephthalate resin for extrusion and injection molding. It has been developed for consideration into applications such as part.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Temperature 23.0 °C |
261000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Crastin® S600F20 NC010 PBT
(Unverified Data**) Crastin® S600F20 NC010 is an unreinforced, lubricated, medium viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Temperature 23.0 °C |
261000 psi @Temperature 73.4 °F |
ISO 899 |
DuPont Performance Polymers Crastin® S600F40 NC010 PBT
(Unverified Data**) Crastin® S600F40 NC010 is an unreinforced, lubricated, low viscosity polybutylene terephthalate resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | ISO 899-1 |
Lanxess Pocan® B 2505 000000 PBT PBT, non-reinforced, injection molding, flame retardant |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Time 3.60e+6 sec |
261000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® FG6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6129 NC010 is an unreinforced high viscosity polybutylene.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Time 3.60e+6 sec |
261000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® FG6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced High Viscosity Polybutylene Terephthalate Developed for Food Contact Applications and Extrusion and Injection Molding Crastin FG6130 NC010 is an unreinforced medium high viscosity polyb.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Time 3.60e+6 sec |
261000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Time 3.60e+6 sec |
261000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Time 3.60e+6 sec |
261000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® S600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Low Viscosity Polybutylene Terephthalate Crastin S600F40 NC010 is an unreinforced lubricated low viscosity polybutylene terephthalate resin for injection molding.Information provided by.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Time 3.60e+6 sec |
261000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® S620F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S620F20 NC010 is an unreinforced nucleated lubricated medium viscosity polybutylene terephthalate resin for fast injection molding.In.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa @Time 3.60e+6 sec |
261000 psi @Time 1000 hour |
ISO 899-1 |
DuPont Performance Polymers Crastin® S650FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)< Unreinforced Flame Retardant Polybutylene Terephthalate Crastin S650FR is an unreinforced flame retardant polybutylene terephthalate for injection molding.Information provided by DuPont Performance .. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
BASF Polystyrol® 427 D Impact Grade Polystyrene (Europe) Heat distortion resistant, easy flowing, rapid freezing, low-impact grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
BASF Polystyrol® 432 B Impact Grade Polystyrene (Europe) Very easy-flowing, low impact grade for parts with unfavorable flow path/wall-thickness ratios.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
Arkema Group Altuglas® GR 7E LIL Acrylic ALTUGLAS GR 7E LIL is an injection molding grade with excellent balance between mechanical, thermal and optical properties.Key features : easy processing and demolding improved chemical resistance .. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
Arkema Group Altuglas® 84 L Acrylic-Styrene Copolymer ALTUGLAS 84 L is a new type of acrylic polymer produced by ATOHAAS which increases the range of material for injection molding applications. ALTUGLAS 84 L is a styrene methylmethacrylate copolymer s.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
Arkema Group Oroglas® V 044 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 044 is an extrusion grade offering good compromise between physical properties and thermal resistance.OROGLAS V 044 is recommended for extrusion of profiles, tubes and sheets.ISO data prov.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
Arkema Group Oroglas® V 045 Acrylic, Extrusion Grade
(discontinued **) OROGLAS V 045 is a lubricated extrusion grade offering good combination of physical and optical properties.OROGLAS V 045 provides easy processing behavior.OROGLAS V 045 is recommended for extrusion.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
Arkema Group Oroglas® V 825 HID Acrylic, UV, Heat Resistant
(discontinued **) OROGLAS HID is an acrylic resin formulated to withstand continuous exposure to high intensity discharge ( HID ) sources up to 90°c.Above 80°c, OROGLAS V 825 HID resin retains its original appearan.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
Arkema Group Oroglas® V 825 T Acrylic
(discontinued **) OROGLAS V 825 T exhibits an excellent balance of properties including superior thermal resistance with an easy processing behavior.OROGLAS V 825 T is then the material of choice for automotive appli.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
Arkema Group Oroglas® V 920 Acrylic, Injection Molding Grade
(discontinued **) OROGLAS V 920 is an injection molding grade with a good balance of properties :Superior flow with medium thermal resistance.The processing of OROGLAS V 920 is easy in terms of injection molding, mo.. |
|||
Tensile Creep Modulus, 1000 hours | 1800 MPa | 261000 psi | |
Arkema Group Oroglas® V 920 T Acrylic, Injection Molding Grade
(discontinued **) OROGLAS V 920 T is an injection molding grade with an improved thermal resistance HDT A ( 1.82 MPa ) = 96°c without any adverse effect on mechanical and optical properties.The processing of OROGLAS.. |