Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.351 - 0.526 N/tex | 3.98 - 5.96 g/denier | |
EMS-Griltech Grilon® BM 10 Nylon 6 Monofilament (Medium-Set) Description: GRILON BM 10 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |
|||
Tenacity | 0.439 - 0.526 N/tex | 4.97 - 5.96 g/denier | |
EMS-Griltech Grilon® BM 20R Nylon 6 Monofilament (Medium-Set) Description: GRILON BM 20R is a Nylon 6 based monofilament for press felt fabric and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |
|||
Tenacity | 0.439 - 0.526 N/tex | 4.97 - 5.96 g/denier | |
EMS-Griltech Grilon® BN 19 Nylon 6 Monofilament (Non-Set) Description: GRILON BN 19 is a Nylon 6 based monofilament for filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |
|||
Tenacity | 0.351 - 0.526 N/tex | 3.98 - 5.96 g/denier | |
EMS-Griltech Grilon® BN 20R Nylon 6 Monofilament (Non-Set) Description: GRILON BN 20R is a Nylon 6 based monofilament for press felt fabric and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provided by EMS-Griltech. |