Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.441 N/tex | 5.00 g/denier | |
Shakespeare Resistat® F901 A013 Nylon 66 Monofilament Resistat F901, MERGE A013 is a .13 millimeter nylon 6,6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickn.. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | 2 kg breaking load |
Shakespeare Sanstat® CN125 .21mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | 9.7 kg breaking load |
Shakespeare Sanstat® CN125 .52mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | 14.5 kg breaking load |
Shakespeare Sanstat® CN125 .64mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | 7 kg breaking load |
Shakespeare Sanstat® CN125 .41mm Nylon 66 Monofilament Sanstat CN125 nylon 6,6 monofilaments have electrically conductive carbon suffused into the surface. The filaments have a carbon coating thickness of approximately 1 micron.Information provided by .. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | |
Shakespeare Resistat® F901 J022 Nylon 66 Monofilament Resistat F901, MERGE J022 is a 22-denier nylon 6,6 monofilament which has electrically conductive carbon suffused into the surface. The filament has a round cross section with a coating thickness o.. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | Knot Strength |
UBE 1022T Nylon 6 Monofilament (Drawing Ratio=5) Specialties: Medium viscosity Nylon 6 Homopolymer Applications: Fishing net, Small size monofilament, General applicationInformation provided by UBE. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | Knot Strength |
UBE 5021T Nylon 6/66 Monofilament (Drawing Ratio=4.5) Specialties: Medium viscosity Nylon 6/66 Copolymer, High knot strength (for Knot improvement), Softness is similar with 1022MT2 (At the heat setting of the net, higher shrink ratio may be expected t.. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | at break; ASTM D638 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | at break; ASTM D638 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | at break; ASTM D638 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | at break; ASTM D638 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | at break; ASTM D638 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | at break; ASTM D638 |
A. Schulman PP 3491 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3491 is a low water carry over homopolymer polypropylene, designed for high speed extrusion.Information provided by A. Schulman. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | Straight test - filament yarn tested at 3 TPI, 10 inch gauge length and 60%/min extension rate. DuPont Test Method 12002 |
DuPont™ Nomex® 430 1200 Denier Aramid Yarn A high crystallinity natural filament yarn of NOMEX with higher strength and chemical resistance than staple spun yarns. Type 430 is used where the aesthetics and properties of a filament yarn are .. |
|||
Tenacity | 0.441 N/tex | 5.00 g/denier | |
Shakespeare NX-301 Nylon 66 Monofilament Produced from a heat stabilized, high molecular weight polymer which increases heat and abrasion.Information provided by Shakespeare Company. |