Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.309 N/tex | 3.50 g/denier | ASTM D2256/ASTM D3822 |
NatureWorks® Ingeo™ 6060D Fiber Grade PLA NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech.. |
|||
Tenacity | 0.309 N/tex | 3.50 g/denier | ASTM D2256/ASTM D3822 |
NatureWorks® Ingeo™ 6302D Fiber Grade PLA NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech.. |
|||
Tenacity | 0.309 N/tex | 3.50 g/denier | ASTM D3218 |
Total PPH 3662 Polypropylene Homopolymer, Fiber Grade, for Staple Fiber, Multifilament Yarns and Slit Tape Fading Resistance TOTAL Polypropylene 3662 is formulated to resist gas fading while maintaining excellent processing stabilityProcess Stability. 3662 features excellent processability and the good.. |
|||
Tenacity | 0.309 N/tex | 3.50 g/denier | |
Shakespeare Resistat® F9322 A061 Nylon 6 Monofilament Resistat F9322, MERGE A061 is composed of a 22 denier nylon 6 monofilament, which has electrically conductive carbon suffused into the surface, combined with two ends of 70/30 polyester yarn. The c.. |