Polymer Property : Tenacity = 0.424 N/tex Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tenacity 0.388 - 0.424 N/tex
4.40 - 4.80 g/denier
Intercontinental Polymers Deniers 1.5-2 Polyester Staple Fibers, Deniers 1.5 - 2
Cut Lengths (Inches): 1, 1.25, 1.75, 2, 3 & 4. Lusters: Bright and Semi-Dull. Cross-Section: Round. Specialties: Optical Black, Spun-Dyed Black, Flame Retardant (US and European Standards), Cati..