Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.371 - 0.416 N/tex | 4.20 - 4.71 g/denier | Average value: 0.380 N/tex Grade Count:5 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |