Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.446 - 0.545 N/tex | 5.05 - 6.17 g/denier | |
EMS-Griltech Grilamid® DN 80 Nylon 12 Monofilament Description: GRILAMID Monofilaments are mainly used in Filtration. Data provided by EMS-Griltech. |