Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tenacity | 0.370 - 0.509 N/tex | 4.19 - 5.77 g/denier | Average value: 0.447 N/tex Grade Count:3 |
Overview of materials for Nylon 610 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Tenacity | 0.370 N/tex | 4.19 g/denier | GB/T14337-2008 |
Sichuan Deyang Haton® 5.5 dtex Polyphenylene Sulfide Staple Fiber Excellent chemical stabilityInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Tenacity | 0.370 - 0.463 N/tex | 4.19 - 5.25 g/denier | |
EMS-Griltech Grilon® XA 136 Nylon 610 Monofilament (Super-Set) Description: GRILON XA 136 is a Nylon 610 based monofilament for paper machine, clothing, forming screen, and filtration.Special Note: GRILON Monofilament has been bought by ShakespeareData provid.. |