Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 112 °C @Thickness 1.20 mm |
234 °F @Thickness 0.0472 in |
|
LyondellBasell Adsylâ„¢ 3 C 30 F HP Polypropylene Copolymer Description: Adsylâ„¢ 3 C 30 F HP is a new alpha olefin modified polypropylene copolymer especially designed for Bopp Film technology. The grade is formulated with a general purpose stabilization.. |
|||
Heat Seal Strength Initiation Temperature | 112 °C | 234 °F | 1.2 mil |
LyondellBasell Adsylâ„¢ 3 C 37 F HP Polypropylene Copolymer Description: Adsylâ„¢ 3 C 37 F HP is a new alpha olefin modified polypropylene copolymer especially designed for Bopp Film technology. It contains anti-blocking and slip agents. Adsylâ„¢ 3 C 3.. |
|||
Heat Seal Strength Initiation Temperature | 112 °C | 234 °F | 1.2 mil |
LyondellBasell Adsylâ„¢ 3 C 39 F HP Polypropylene Copolymer Description: Adsylâ„¢ 3 C 39 F HP is a new alpha olefin modified polypropylene copolymer especially designed for Bopp Film technology. It contains anti-blocking agents but no slip agent and is th.. |
|||
Heat Seal Strength Initiation Temperature | 112 °C | 234 °F | Minimum seal strength is 200 g/in at 15 psi pressure and 1 sec.; ASTM D1709 |
Total PPR Z9450 Random Copolymer Heat Sealable Grade ATOFINA Z9450 is a low melting, high ethylene random copolymer with improved color, optics and impact properties. The very low melting point of ATOFINA Z9450 makes it an excellent heat seal layer f.. |
|||
Heat Seal Strength Initiation Temperature | 112 °C | 234 °F | Total Method |
Total Lumicene® mPE M 2710 EP Metallocene Polyethylene, Film Metallocene Medium Density Film ResinCharacteristics:Outstanding clarity and glossExcellent bubble stabilityExcellent tear strengthHigh puncture resistanceGood stiffnessExcellent heat sealing proper.. |