Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 108 °C | 226 °F | 3 N; Borealis Test |
Borealis Borseal™ TD120BF Terpolymer for BOPP Film Borseal TD120BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD120B.. |
|||
Heat Seal Strength Initiation Temperature | 108 °C | 226 °F | 2 N; Borealis Test |
Borealis Borseal™ TD220BF Terpolymer for BOPP Film Borseal TD220BF is a C2/C4 terapolymer film resin especially developed for use as sealing layers in coextruded BOPP film (manufactured on stenter frame and double bubble film process).Borseal TD220B.. |