Polymer Property : Heat Seal Strength Initiation Temperature = 191 °C Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 135 - 191 °C
275 - 375 °F
1 sec @40 psi
DuPont Teijin Films Melinex® 3381 Polyester Film
Melinex® 3381 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well a..
Heat Seal Strength Initiation Temperature 135 - 191 °C
275 - 375 °F
1 sec @40 psi
DuPont Teijin Films Melinex® 342 Polyester Film
Melinex® 342 is a two-side heat-sealable, clear polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well as a vari..
Heat Seal Strength Initiation Temperature 135 - 191 °C
275 - 375 °F
1 sec @40 psi
DuPont Teijin Films Melinex® 357 Polyester Film
Melinex® 357 is a two-sided heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well a..