Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 94.0 °C | 201 °F | 1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method |
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP) AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g.. |