Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 157 °C | 315 °F | 0.40 lb/in heat seal strength; SWTM-19 |
Dow SARAN WRAP™ 3 Plastic Film SARAN WRAP™ 3 Plastic Film is a clear biaxially oriented monolayer barrier film, designed for tight wrap and heat sealing applications. It is available in 50 gauge, as single or double would rolls.. |