Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 123 °C
253 °F
Hyosung Topilene C600H PP
C600H Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Very low sealSlip propertyTransparencyInformation provided by Hyosung Corporation