| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1601B Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601B is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, se.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1652-1 Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating
(discontinued **) Surlyn® 1652-1 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® NWL Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® NWL is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Film produced from this resin is .. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1601-2 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1601-2LM Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1601-2LM (Low Moisture) is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications:.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1605 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1605 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1650 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1650 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1652 Zinc Ionomer Resin for Flexible Packaging Surlyn® 1652 is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene .. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1857 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1857 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1901 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 1901 is a sodium ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultr.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1652SB Zinc Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1652SB is an ionomer resin available for use in blown/cast film and extrusion coating operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylen.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1705-1 Zinc Ionomer Resin for Blown and Cast Film Surlyn® 1705-1 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, s.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1802 Sodium Ionomer Resin for Blown/Cast Film and Extrusion Coating Surlyn® 1802 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment and extrusion coating and coextrusion coating equipment designed to proces.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 2601 Sodium Ionomer Resin for Blown and Cast Film Surlyn® 2601 is an ionomer resin available for use in blown and cast film operations. It can be used in both extrusion and coextrusion equipment designed to process polyethylene resins. Applicati.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | Average value: 0.0450 GPa Grade Count:17 |
| Overview of materials for Ionomer, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
| Secant Modulus, TD | 0.0450 GPa | 6.53 ksi | ASTM D882 |
| DuPont™ Surlyn® 1601B-2 Sodium Ionomer Resin for Blown and Cast Film
(discontinued **) Surlyn® 1601 B-2 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry,.. |
|||