Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 4.21 GPa | 610 ksi | ASTM D882A |
DuPont Teijin Films Melinex® 606 Polyester Film, 300 Gauge Melinex® 606 is a very smooth two-side coated polyester film designed specifically for high density floppy disks.Also available in 285 GaugeInformation provided by DuPont. |
|||
Secant Modulus, TD | 4.21 GPa | 610 ksi | ASTM D882A |
DuPont Teijin Films Mylar® ADS Polyester Film, 300 Gauge Mylar® ADS is a heat stabilized, low shrinkage film with good web handling properties. Approvals: UL 94 VTM-2 - for 92 - 500 gauge (0.023 - 0.13mm)Also available in 285 GaugeInformation provided by.. |