Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.304 GPa | 44.1 ksi | 2% Secant; ASTM D882 |
LyondellBasell Adflexâ„¢ Q 401 F TPO Resin Thermoplastic olefin resin wit slip and antiblock for air quenched blown film, excellent heat resistance, excellent puncture resistance, great tear resistance, FDA acceptableApplications: films requ.. |