Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y826-CP Hexene LLDPE Film Resin Film Properties. Features: Good stiffness, intended for narrow die gaps, high strength and toughness.Applications: Industrial bags, industrial packaging.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: slip, antiblock, and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blendedApplications: thick .. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
Chevron Phillips Vytek™ V205E9 Enhanced LLDPE Blown Film Resin
(discontinued **) Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
Chevron Phillips MarFlex® 5355 LDPE Industrial Clarity, General Purpose Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Suited for High Speed Converting, Good Impact Strength, Excellent Processability, Good Sealability, Good OpenabilityApplications:Institutional Packaging, Food.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
Chevron Phillips 5455 LDPE Clear, General Purpose Packaging Film Resin
(discontinued **) Resin Type: HomopolymerCharacteristics: Good Clarity, High Gloss, Good Openability, Good Sealability, Suited for High Speed ConvertingApplications:Bakery and Food Products, Rack and Counter Merchand.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
ExxonMobil Escorene® LD-104 LDPE Packaging Film Resin, High Clarity
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer packaging film resin with excellent clarity and good stiffness. It is excellent either blown film or chill roll casting equipment. I.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
ExxonMobil Escorene® LD-134 LDPE Packaging Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer film resin with good clarity. It is suitable for processing in blown film equipment and can be drawn down to 1.0 mil.Applications: Fo.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y826-D Hexene LLDPE Film Resin Film Properties. Features: High strength and toughness, excellent puncture resistance, good stiffness and machinability.Applications: Premium trash bags, bags-on-roll.Data provided by the manufactu.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD2305F Low Density Polyethylene Film Key Characteristics:Excellent clarity and glossGood zip formationContains 1000 ppm slip agent and 500 ppm antiblocking agentRecommended Applications:Zip bagsGeneral purpose film for food packagingIn.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ISO 527-3 |
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal.. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
NOVA Chemicals Sclair® 11E1 Butene LLDPE Film Resin
(discontinued **) Film Properties. Features: Low gel, strength and toughness.Applications: Base resin.Data provided by the manufacturer. |
|||
Secant Modulus, TD | 0.250 GPa | 36.3 ksi | ASTM D882 |
NOVA Chemicals Novapol® TF-Y826-BP Hexene LLDPE Film Resin
(discontinued **) Film Properties. Features: Good stiffness and machinability, intended for narrow die gaps, high strength and toughness.Applications: Grocery sacks, boutique bags, frozen food packaging.Data provide.. |
|||
Secant Modulus, TD | 0.250 - 0.772 GPa | 36.3 - 112 ksi | Average value: 0.447 GPa Grade Count:5 |
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and .. |