Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.214 GPa | 31.0 ksi | ASTM D882 |
Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin Resin Type: Hexene CopolymerCharacteristics: Good OpticsGood drawdownExcellent processabilityCan use straight or in blends with LDPE or HDPEApplications: Bakery filmsOverwrapCoextrusionsInformation .. |
|||
Secant Modulus, TD | 0.214 GPa | 31.0 ksi | Film value |
Dow AFFINITY™ HF 1030 Polyolefin Plastomer AFFINITY® HF 1030 polyolefin plastomer is an ethylene alpha-olefin resin designed to provide cast embossed film products with high modulus for machinability, excellent drawdown at high line speeds,.. |