Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 1.90 GPa | 276 ksi | ASTM D882 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Secant Modulus, TD | 1.90 GPa | 276 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® EF-F Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 32 mol % Ethylene. Non oriented type film; property values for 15 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pro.. |
|||
Secant Modulus, TD | 1.90 GPa | 276 ksi | Youngs Modulus, ASTM D638, 10%/min. |
EVALCA EVAL® EF-E Ethylene Vinyl Alcohol Copolymer Film
(discontinued **) 44 mol % Ethylene. Non oriented type film; property values for 20 µm film.Data provided by EVALCA. Applications: EVOH is used in packaging applications because of its outstanding gas barrier pr.. |