Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.169 GPa | 24.5 ksi | ASTM D882 |
Huntsman PE1356 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Secant Modulus, TD | 0.169 GPa | 24.5 ksi | ASTM D882 |
Huntsman PE1335 EVA Film Extrusion
(discontinued **) 3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Secant Modulus, TD | 0.169 GPa | 24.5 ksi | ASTM D882 |
Huntsman PE1345 EVA Film Extrusion
(discontinued **) 3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Secant Modulus, TD | 0.169 GPa | 24.5 ksi | ASTM D882 |
Huntsman PE 1375 EVA Film Extrusion
(discontinued **) 3.7% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Secant Modulus, TD | 0.169 GPa | 24.5 ksi | ASTM D882 |
Huntsman PE1353 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |