Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.137 GPa | 19.9 ksi | ASTM D882 |
ExxonMobil Exceed™ 357C32 LDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 357C32 resin have outstanding tensile properties and.. |