Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Secant Modulus, TD = 16.7 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.115 GPa
16.7 ksi
5%; ASTM D882
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend
The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en..
Secant Modulus, TD 0.115 GPa
16.7 ksi
ASTM D882
Huntsman PE1651 EVA Film Extrusion  (discontinued **)
6.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Yields film with outstanding low temperature strength, excellent clarity, and good heat seal.Applications: Film extrusion: ice bags, liqui..
Secant Modulus, TD 0.115 GPa
16.7 ksi
2% Secant; ASTM D882
Dow AFFINITY™ PL 1850G Polyolefin Plastomer (POP)
AFFINITY™ PL 1840G Polyolefin Plastomer (POP) is produced via INSITE™ Technologies. It is designed to provide blown and cast film products with low temperature sealability, excellent optics and g..
Copyright © lookpolymers.com All Rights Reserved