Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.104 GPa | 15.1 ksi | ASTM D882 |
Huntsman PE1903 EVA Film Extrusion
(discontinued **) 9% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent toughness and flexibility at low temperatures, and good heat-seal response.Applications: Film extrusion: laminating film, controll.. |