Polymer Property : Secant Modulus, TD = 0.317 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.317 GPa
46.0 ksi
ASTM D882
ExxonMobil Escorene® LL-3105 LLDPE/Hexene Premium Film Resin, Tough, 1.2 mil film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3105 have outstanding tensile and toughness properties. The superior strength propert..
Secant Modulus, TD 0.317 GPa
46.0 ksi
1% Strain; ASTM D882
M. Holland Company LL102 LLDPE  (discontinued **)
Additives: Medium Antiblock, Medium SlipFeatures: Medium Antiblocking, Butene Comonomer, Copolymer, Good Drawdown, Good Processability, Medium SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c)..
Secant Modulus, TD 0.317 GPa
46.0 ksi
ASTM D882
ExxonMobil Exceed™ 377D60 LDPE/Hexene Tough Premium Film Resin, 3 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A hexene copolymer produced using Exxon Chemical's EXXPOL® technology. Films made from EXCEED 377D60 resin exhibit excellent impact strength and b..
Secant Modulus, TD 0.317 GPa
46.0 ksi
2% Secant; ASTM D882
Dow INTEGRAL™ 932 High Heat Multilayer Adhesive Film
INTEGRAL 925 High Heat Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, fiberglass, non-wovens,..
Secant Modulus, TD 0.317 GPa
46.0 ksi
1% Strain; ASTM D882
M. Holland Company LL106 LLDPE  (discontinued **)
Additives: Antiblock, SlipFeatures: Unspecified Antiblocking, Hexane Comonomer, Copolymer, Good Drawdown, Good Processability, Unspecified SlipUses: Film, LinersApprovals: FDA 21 CFR 177.1520(c) 2.2..