Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.274 GPa | 39.7 ksi | 1% Secant; ASTM D882 |
Eastman 1810F Polyethylene
(discontinued **) Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt.. |
|||
Secant Modulus, TD | 0.274 GPa | 39.7 ksi | 1% Secant; ASTM D882 |
Eastman D4004-F Polyethylene
(discontinued **) Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o.. |
|||
Secant Modulus, TD | 0.274 GPa | 39.7 ksi | 1% Secant; ASTM D882 |
Eastman D4008-F Polyethylene
(discontinued **) Polyethylene D4008-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness and clarityList of Applications: Food packagingFood-contac.. |
|||
Secant Modulus, TD | 0.274 GPa | 39.7 ksi | 1% Secant; ASTM D882 |
Eastman E6838-969F Polyethylene
(discontinued **) E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap... |
|||
Secant Modulus, TD | 0.274 GPa | 39.7 ksi | 1% Secant; ASTM D882 |
Eastman D4052-F Polyethylene
(discontinued **) D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance... |
|||
Secant Modulus, TD | 0.274 GPa | 39.7 ksi | 1% Secant; ASTM D882 |
Eastman E6838-975F Polyethylene
(discontinued **) E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film.. |