Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Medium Slip, High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE. S.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Antiblock, Process Aid Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPE. Slip 0 ppm. Antiblock.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 6120 LLDPE Cast/Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Optics, Good Drawdown, Can be used straight or blended with LDPE or HDPE, Can be used in blown or cast applicationsAp.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L1810F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesContains 1600 ppm slip agent and 1900 ppm antiblocking agentRecommended Applications:Film for heavy duty bag, industrial bag, rice bag, su.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L1810FI Linear Low Density Polyethylene Film Key Characteristics:High gloss and clarityContains 3200 ppm slip agent and 2400 ppm antiblocking agentRecommended Applications:Water-quench blown film for general purpose bags such as vegetable or f.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2009F Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains 1000 ppm slip agent and 700 ppm antiblocking agentR.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ L2009FA Linear Low Density Polyethylene Film Key Characteristics:High productivityGood optical propertiesCan be blended with HDPE and LDPE to improve tear resistance and seal strengthContains no slip agent and antiblocking agentRecommended App.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1902F Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactContains 1400 ppm slip content and 2400 ppm antiblocking contentRecommended Applications:G.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
SCG Chemicals EL-Leneâ„¢ LD1902FA Low Density Polyethylene Film Key Characteristics:High strengthGood optical propertiesCan be blended with HDPE, LLDPESafe for food contactRecommended Applications:General purpose bag, big bagMedium-weight shrink filmInformation .. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882-A |
Borealis Himod™ FT5270 LDPE for Film Himod FT5270 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industr.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 7105DKT LLDPE Blown Film Resin, Hexene Copolymer
(discontinued **) Resin Type: Hexene Copolymer, High Antiblock, Processing Aid Version of 7105T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags.. |
|||
Secant Modulus, TD | 0.270 GPa | 39.2 ksi | ASTM D882 |
Chevron Phillips 6109M LLDPE Blown Film Resin, Butene Copolymer
(discontinued **) Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE... |