Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.179 GPa | 26.0 ksi | 1% Secant; ASTM D882 |
Eastman D4028-F Polyethylene
(discontinued **) D4028-F is a low density formulation which contains high antiblock. It is suggested for film applications that require reasonable clarity. D4028-F meets the requirements of FDA regulations at 21 CF.. |
|||
Secant Modulus, TD | 0.179 GPa | 26.0 ksi | 1% Secant; ASTM D882 |
Eastman E6838-014F Polyethylene
(discontinued **) E6838-014F is a low density formulation that contains low slip and medium antiblock levels. It is suggested for film applications that require clarity.List of Applications: Food packagingFood-conta.. |
|||
Secant Modulus, TD | 0.179 GPa | 26.0 ksi | ASTM D882 |
Chevron Phillips MarFlex® 5628 LDPE Blown Film Resin Resin Type: HomopolymerCharacteristics: Superior tensile and impact strengthGood abrasion and tear resistanceExcellent retention of properties after agingApplications: LaminationsPallet shrinkcase s.. |
|||
Secant Modulus, TD | 0.179 GPa | 26.0 ksi | 0.1 mm/mm-min Initial Strain Rate; ASTM D-882 |
Bapolene® 105F Low Density Polyethylene Film Resin Description: Bapolene LD105F is an unmodified low density polyethylene which extrudes into a low gloss high impact film. It contains antiblock additives and no slip additives. This product meets th.. |