Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.172 GPa | 24.9 ksi | 1% Secant; ASTM D882 |
Westlake Mxsten CV CV77515-F Plastomer
(discontinued **) Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s.. |
|||
Secant Modulus, TD | 0.172 - 1.37 GPa | 25.0 - 199 ksi | Average value: 0.504 GPa Grade Count:13 |
Overview of materials for Medium Density Polyethylene (MDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Film Grade". Each property range of values reported is minimum and m.. |
|||
Secant Modulus, TD | 0.172 GPa | 24.9 ksi | ASTM D882 |
LyondellBasell Montell 16502F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Secant Modulus, TD | 0.172 GPa | 24.9 ksi | ASTM D882 |
LyondellBasell Montell 16502F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Secant Modulus, TD | 0.172 GPa | 24.9 ksi | ASTM D882 |
LyondellBasell Montell 16502F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Secant Modulus, TD | 0.172 - 0.228 GPa | 25.0 - 33.0 ksi | Average value: 0.193 GPa Grade Count:3 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Secant Modulus, TD | 0.172 GPa | 24.9 ksi | ASTM D882 |
ExxonMobil Escorene® LD-331 EVA Film Resin, Very High Clarity, Very High Impact
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 5.8% vinyl acetate copolymer, high clarity film resin. Film made from this resin exhibits superior impact strength and heat sealability.Applicati.. |