Mechanical Properties Metric English Comments
Secant Modulus, TD 0.169 GPa
24.5 ksi
ASTM D882
Huntsman PE1356 EVA Film Extrusion  (discontinued **)
3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Secant Modulus, TD 0.169 GPa
24.5 ksi
ASTM D882
Huntsman PE1335 EVA Film Extrusion  (discontinued **)
3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Secant Modulus, TD 0.169 GPa
24.5 ksi
ASTM D882
Huntsman PE1345 EVA Film Extrusion  (discontinued **)
3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Secant Modulus, TD 0.169 GPa
24.5 ksi
ASTM D882
Huntsman PE 1375 EVA Film Extrusion  (discontinued **)
3.7% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Secant Modulus, TD 0.169 GPa
24.5 ksi
ASTM D882
Huntsman PE1353 EVA Film Extrusion  (discontinued **)
3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: ..
Copyright © lookpolymers.com All Rights Reserved