Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, TD | 0.159 GPa | 23.1 ksi | ASTM D882 |
ExxonMobil Escorene® LL-3023 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3023 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Secant Modulus, TD | 0.159 GPa | 23.1 ksi | 2% Secant; ASTM D882 |
Dow DAF 780 Carpet Underlayment Adhesion Film DAF 780 is a low melt point, coextruded film used to improve slip characteristics of polyurethane foam for carpet installation or other applications.Information provided by Dow |
|||
Secant Modulus, TD | 0.159 GPa | 23.1 ksi | ASTM D882 |
ExxonMobil Escorene® LL-3003 LLDPE/Hexene Premium Cast Stretch Film Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3003 have outstanding tensile properties as well as stiffness and toughness.Applicatio.. |
|||
Secant Modulus, TD | 0.159 GPa | 23.1 ksi | ASTM D882 |
Huntsman Rexell® L8102 Cast Film Extrusion LLDPE
(discontinued **) Linear-low density copolymer with high slip and medium antiblock, general purpose blown film extrusion, FDA compliant.Features: Excellent combination of sealability, mechanical strength and optics.A.. |
|||
Secant Modulus, TD | 0.159 GPa | 23.1 ksi | ASTM D882 |
Huntsman PE1403 EVA Film Extrusion
(discontinued **) 4% Vinyl Acetate EVA Copolymer, DMF listed and FDA compliantFeatures: High clarity film with good toughness and flexibility at low temperatures.Applications: Film extrusion: frozen food and general .. |