Mechanical Properties Metric English Comments
Secant Modulus, TD 0.103 GPa
14.9 ksi
5%; ASTM D882
Petroquimica Triunfo Trithene® TS 7035 LDPE - Film - Lamination and Plastification
The Trithene TS 7035 resin is a low-density polyethylene (LDPE) with an excellent processability, which allows for a low energy consumption during extrusion and warrants the production of thin films..