Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.552 - 0.648 GPa | 80.1 - 94.0 ksi | ASTM D882 |
Honeywell PMP Polymethylpentene Film
(discontinued **) PMP is a clear, red, or blue film manufactured from polymethylpentene. It provides more toughness and heat resistance than standard polyolefins for release film applications.Information provided by.. |