Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.862 - 1.207 GPa | 125 - 175.1 ksi | ASTM D882 |
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Secant Modulus, MD | 0.862 - 1.207 GPa | 125 - 175.1 ksi | ASTM D882 |
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Secant Modulus, MD | 0.862 - 1.207 GPa | 125 - 175.1 ksi | ASTM D882 |
Honeywell ACLAR® 22C (3.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Secant Modulus, MD | 0.676 - 1.207 GPa | 98.0 - 175.1 ksi | ASTM D882 |
Honeywell Capran® K Coated Nylon Film
(discontinued **) Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil.. |
|||
Secant Modulus, MD | 0.676 - 1.207 GPa | 98.0 - 175.1 ksi | ASTM D882 |
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove.. |