Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.6550 GPa | 95.00 ksi | 2% Secant; ASTM D882 |
Dow Saran® 560 Clear Plastic Barrier Film Saran™ 560 is a clear biaxially oriented monolayer barrier film, designed for unit packaging and other applications. It is available in 6 gauge.Information provided by Dow |