Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.517 GPa | 75.0 ksi | ASTM D882 |
Honeywell Capran® 512 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 512 LL is a heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other high temperature .. |
|||
Secant Modulus, MD | 0.517 GPa | 75.0 ksi | ASTM D882 |
Honeywell Capran® 518 LL Heat Stabilized Nylon Film
(discontinued **) Description: Capran® 518 LL is a green tinted, heat-stabilized blown film produced from low lactam nylon-6 resin. It is recommended as bagging film for advanced composite fabrication and other hig.. |