Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 2.758 - 3.889 GPa | 400.0 - 564.1 ksi | ASTM D882 |
Honeywell Capran® Emblem™ 1000 Bi-Axially Oriented Nylon 6 Film Description: Capran® Emblem™ 1000 is a 0.40 mil (10 micron) biaxially oriented nylon 5 film with excellent flex crack resistance and superior clarity properties. Applications: packaging appl.. |
|||
Secant Modulus, MD | 2.758 - 3.999 GPa | 400.0 - 580.0 ksi | ASTM D882 |
Honeywell Capran® Oxyshield™ OBS Monoaxially Oriented, Co-Extruded Nylon 6/EVOH/Nylon 6 Clear Film Description: Oxyshield™ Oriented Barrer is a 0.60 mil (15 micron) monoaxially oriented, co-extruded nylon 6/EVOH/nylon 6 clear film with slip additive having excellent gas barrier through a bro.. |