Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | 1% Secant; ASTM D882 |
Eastman 1830F Polyethylene
(discontinued **) Polyethylene 1830F is a low-density formulation with no slip or antiblock. It is suggested for film applications requiring high clarity, good tear and impact strength, a wide heat sealing range and.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | 1% Secant; ASTM D882 |
Eastman E6838-922F Polyethylene
(discontinued **) E6838-922F is a low density formulation with medium slip and medium antiblock. Outstanding optical properties make this material an excellent choice for food packaging applications.List of Applicat.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-102 LDPE Drawdown Resin, 0.5 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A homopolymer, good clarity, laundry and dry cleaning film resin capable of providing a tough film in very thin gauges.Applications: Dry cleaning es.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | ASTM D882 |
Huntsman PE1031 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | ASTM D882 |
Huntsman PE1044 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and machinability.Applications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms to FDA reg.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | ASTM D882 |
Huntsman PE1055 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Yields film with excellent optical and draw down characteristicsApplications: Film extrusion: soft goods and other high clarity packaging.FDA Notes: Conforms.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | 2% Secant; ASTM D882 |
Dow INTEGRAL™ 925 High Heat Multilayer Adhesive Film INTEGRAL 925 High Heat Adhesive Film is a heat-activated, thermally stable adhesive film for automotive applications capable of bonding to urethane foam-baked fabrics, paper, fiberglass, non-wovens,.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | ASTM D882 |
ExxonMobil Escorene® LL-3002 LLDPE/Hexene Premium Cast Stretch Film Resin, 1.2 mil Film
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A hexene copolymer LLDPE cast film resin. Films made from LL-3002 have outstanding tensile properties as well as stiffness and toughness. These su.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | ASTM D882 |
Huntsman PE1061 Film Extrusion Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink.. |
|||
Secant Modulus, MD | 0.207 GPa | 30.0 ksi | ASTM D882 |
Huntsman PE1158 EVA Film Extrusion
(discontinued **) 1.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |