Mechanical Properties Metric English Comments
Secant Modulus, MD 0.110 GPa
16.0 ksi
5%; ASTM D882
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend
The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en..
Secant Modulus, MD 0.110 GPa
16.0 ksi
ASTM D882
Eastman 5265 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Good optical properties, Superior impact strength, Low coefficient of friction, Good processability, High Slip, High Ant..
Secant Modulus, MD 0.110 GPa
16.0 ksi
ASTM D882
Eastman 5267 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent heat seal characteristics, Excellent impact strength, Good optical properties, Good processability, High antiblock, No slipApplications:Laminations..
Secant Modulus, MD 0.110 GPa
16.0 ksi
ASTM D882
Eastman 5269 LDPE 6.5% EVA Copolymer, Clarity, Ultra-high Impact Film Resin  (discontinued **)
Resin Type: CopolymerCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flow for Injection Blow Molding Applications, Good Par..
Secant Modulus, MD 0.110 GPa
16.0 ksi
ASTM D882
Eastman 5282 LDPE 8% EVA Copolymer, High Clarity, High Impact Film Resin  (discontinued **)
Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, Low Slip, High Antiblock, Good Bubble Stability at High Draw Down Speeds..
Secant Modulus, MD 0.110 GPa
16.0 ksi
ASTM D882
Eastman 5284 LDPE 8% EVA Copolymer, High Clarity, Ultra-High Impact Film Resin  (discontinued **)
Resin Type: CopolymerCharacteristics: Excellent Heat Seal Characteristics, Superior Impact Strength, Good Optical Properties, No Slip, High Antiblock, High Coefficient of FrictionApplications:Ice Ba..
Secant Modulus, MD 0.110 GPa
16.0 ksi
ASTM D882
ExxonMobil Escorene® LD-336 EVA Film Resin, Clarity, Very High Drawdown  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer blown film resin capable of very high drawdown with excellent clarity.Applications: Very thin heat seal layers; Light..
Secant Modulus, MD 0.110 GPa
16.0 ksi
ASTM D882
Huntsman Rexell® L3106 Blown Film Extrusion LLDPE  (discontinued **)
Linear-low density copolymer, cast film extrusion, FDA compliant.Features: Excellent processability with good sealing and optical properties.Applications: Blending resin and general purpose packagin..