Mechanical Properties Metric English Comments
Secant Modulus, MD 0.862 - 1.207 GPa
125 - 175.1 ksi
ASTM D882
Honeywell ACLAR® 22C (10.0 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Secant Modulus, MD 0.862 - 1.207 GPa
125 - 175.1 ksi
ASTM D882
Honeywell ACLAR® 22C (7.50 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Secant Modulus, MD 0.862 - 1.207 GPa
125 - 175.1 ksi
ASTM D882
Honeywell ACLAR® 22C (3.00 mil) Copolymer Film  (discontinued **)
Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe..
Secant Modulus, MD 0.676 - 1.207 GPa
98.0 - 175.1 ksi
ASTM D882
Honeywell Capran® K Coated Nylon Film  (discontinued **)
Description: Capran® K is a PVdc coated nylon 6 film designed for food packaging applications where longer shelf life is required. This film exhibits good clarity, gloss, toughness, thermoformabil..
Secant Modulus, MD 0.676 - 1.207 GPa
98.0 - 175.1 ksi
ASTM D882
Honeywell Capran® Nylon Film, Multipurpose Nylon 6 Film
Description: Capran® is a multipurpose nylon 6 film. Its physical properties are evenly distributed for optimum performance giving excellent resistance to flex cracking. It can be processed ove..