Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.6067 GPa | 88.00 ksi | 2% Secant; ASTM D882 |
Dow Saran® 28 Clear Plastic Barrier Film Saran™ 28 is a clear biaxially oriented monolayer barrier film, designed for chub packaging machines and laminations. It is available in 100 gauge, as single or double wound rolls.Information prov.. |