Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.5330 GPa | 77.30 ksi | 2% Secant; ASTM D882 |
Dow Saran® 560 Vapor Retarder Film Saran™ Vapor Retarder Film is a biaxially oriented barrier film designed as a water vapor retarder for insulation applications. It is available in 600 gauge. Roll size: 35.5" x 250 long.Informat.. |