Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, Medium Slip, High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE. S..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE...
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, High Antiblock, Process Aid Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPE. Slip 0 ppm. Antiblock..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Stretch Wrap, CoextrusionsProcessing Conditio..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips Vytek™ V205C3 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: slip, antiblock, and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be used straight or blendedApplications: thick ..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips Vytek™ V205C6 Enhanced LLDPE Blown Film Resin  (discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
NOVA Chemicals Sclair® 11F2 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer.
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
NOVA Chemicals Sclair® 11Q4 Butene LLDPE Film Resin  (discontinued **)
Film Properties. Features: Low gel, high clarity, good seal characteristics.Applications: Liquid packaging, specialty blending, general purpose sealant.Data provided by the manufacturer.
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips MarFlex® 5355 LDPE Industrial Clarity, General Purpose Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Suited for High Speed Converting, Good Impact Strength, Excellent Processability, Good Sealability, Good OpenabilityApplications:Institutional Packaging, Food..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 5455 LDPE Clear, General Purpose Packaging Film Resin  (discontinued **)
Resin Type: HomopolymerCharacteristics: Good Clarity, High Gloss, Good Openability, Good Sealability, Suited for High Speed ConvertingApplications:Bakery and Food Products, Rack and Counter Merchand..
Secant Modulus, MD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman 1810F Polyethylene  (discontinued **)
Polyethylene 1810F is a fractional-melt low-density formulation with no slip or antiblock. It is suggested for film applications requiring high impact strength, high tear strength and very good opt..
Secant Modulus, MD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman D4004-F Polyethylene  (discontinued **)
Polyethylene D4004-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness, clarity, high strength, and for blending with LLDPEList o..
Secant Modulus, MD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman D4008-F Polyethylene  (discontinued **)
Polyethylene D4008-F is a fractional melt formulation designed for film applications. It is suggested for applications requiring toughness and clarityList of Applications: Food packagingFood-contac..
Secant Modulus, MD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman E6838-969F Polyethylene  (discontinued **)
E6838-969F is a low density formulation with no slip and medium antiblock. It is suggested for film applications that require toughness such as shrink/bundling film, disposable diapersand overwrap...
Secant Modulus, MD 0.220 GPa
31.9 ksi
1%; ASTM D882
Braskem Flexus® 9210 LLDPE Blown Film Extrusion  (discontinued **)
25µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); multilayer packaging films; films for lamination. Information provided by Braskem
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industr..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 7105DKT LLDPE Blown Film Resin, Hexene Copolymer  (discontinued **)
Resin Type: Hexene Copolymer, High Antiblock, Processing Aid Version of 7105T, Cast/Blown Film ResinCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended wit..
Secant Modulus, MD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman D4052-F Polyethylene  (discontinued **)
D4052-F is a fractional-melt low density formulation with low slip and low antiblock. It is suggested for film applications requiring impact strength, outstanding clarity, and good tear resistance...
Secant Modulus, MD 0.220 GPa
31.9 ksi
1% Secant; ASTM D882
Eastman E6838-975F Polyethylene  (discontinued **)
E6838-975F is a low density formulation with medium slip and medium antiblock. The formula is used in general purpose packaging where impact strength and processability are important. End-use film..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene CopolymerCharacteristics: Good Stiffness at Thin Gauges, Good Drawdown, Can be used straight or blended with LDPE or HDPEApplications:Industrial Liners, Stretch Wrap, Garment Bags..
Secant Modulus, MD 0.220 GPa
31.9 ksi
ASTM D882
Chevron Phillips 6109M LLDPE Blown Film Resin, Butene Copolymer  (discontinued **)
Resin Type: Butene Copolymer, High Slip, Very High Antiblock Version of 6109Characteristics: Good Stiffness at Thin Gauges, Good Drawdown, Low COF, Can be used straight or blended with LDPE or HDPE...
Copyright © lookpolymers.com All Rights Reserved