Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.166 GPa | 24.1 ksi | ASTM D882 |
Huntsman PE 1017 Film Extrusion Polyethylene
(discontinued **) Homopolymer, Drug Master File listed product, and FDA compliant.Features: Good impact strength, good machinability, heat seal and foaming characteristicsApplications: Film Extrusion: industrial line.. |
|||
Secant Modulus, MD | 0.166 GPa | 24.1 ksi | ASTM D882 |
Huntsman PE1023 Film Extrusion Polyethylene
(discontinued **) Homopolymer, and FDA compliant.Features: Good draw down characteristics.Applications: Film extrusion: drum liners, hardware packaging, and refuse bags.FDA Notes: Conforms to FDA regulation 21 CFR 17.. |
|||
Secant Modulus, MD | 0.166 GPa | 24.1 ksi | ASTM D882 |
Huntsman PE1201 EVA Film Extrusion
(discontinued **) 2% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Good optical, medium impact strength, and good processability.Applications: Film extrusion: heavy duty packaging.FDA Notes: Conforms to FDA .. |