Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.162 GPa | 23.5 ksi | 50 µm (2 mil) film; ASTM D882 |
DuPont Nucrel® 403 Ethylene-Methacrylic Acid Copolymer Resin for Blown and Cast Film 4 wt% Methacrylic Acid.Nucrel® 0403 is an ethylene-methacrylic acid copolymer resin available for use in blown and cast film extrusion and coextrusion equipment designed to process polyethylene res.. |