Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | 1% Secant; ASTM D882 |
Westlake Mxsten CV CV77515-F Plastomer
(discontinued **) Mxsten CV plastomer CV77515-X is a polyethylene plastomer designed for blown film extrusion that contains medium slip and no antiblock additives. Films produced with this resin exhibit a very low s.. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
M. Holland Company LD219 LDPE
(discontinued **) Features: Good Processability, Good ToughnessUses: Bottles, Industrial Applications, PackagingProcessing Method: Blow MoldingInformation provided by M. Holland. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
M. Holland Company LD220 LDPE
(discontinued **) Features: Good Heat Seal, Good Processability, Good ToughnessUses: Industrial Applications, Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
ExxonMobil Escorene® LD-141 EVA Shrink Film Resin, FMI
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A fractional melt index, 2.0% vinyl acetate copolymer film resin with very good toughness and shrink properties. The low melt index gives excellent.. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
Huntsman PE1356 EVA Film Extrusion
(discontinued **) 3.5% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
LyondellBasell Montell 16502F3 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, no slip, no antiblockApplications: can liners and trash bags, blends, thin filmsMeets FDA.. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
LyondellBasell Montell 16502F7 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, low slip, medium antiblockApplications: can liners and trash bags, blends, thin filmsMeet.. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
LyondellBasell Montell 16502F8 Butene LLDPE Key Features: butene LLDPE resins for film extrusion applications, easy processing, low gels, good strength, medium slip, high antiblockApplications: can liners and trash bags, blends, thin filmsMee.. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | 1% Secant; ASTM D882 |
M. Holland Company LD220MM LDPE
(discontinued **) Additives: Medium Antiblock, SlipFeatures: Medium Antiblocking, Good Heat Seal, Medium SlipUses: Liners, PackagingProcessing Method: Blown FilmInformation provided by M. Holland. |
|||
Secant Modulus, MD | 0.152 - 0.208 GPa | 22.0 - 30.2 ksi | Average value: 0.177 GPa Grade Count:4 |
Overview of materials for Low Density Polyethylene (LDPE), Blow Molding Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Blow Molding Grade". Each property range of values reported is minimum .. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
Huntsman PE1335 EVA Film Extrusion
(discontinued **) 3.3% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
Huntsman PE1345 EVA Film Extrusion
(discontinued **) 3.4% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
Huntsman PE 1375 EVA Film Extrusion
(discontinued **) 3.7% Vinyl Acetate EVA copolymer and FDA compliantFeatures: Excellent balance of optical and strength, toughness and flexibility at low temperatures, and good heat seal characteristic.Applications: .. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | 1% Secant; ASTM D882 |
Westlake Hifor Xtreme SC74860-F Polyethylene
(discontinued **) Hifor Xtreme Polyethylene SC74860-F is recommended for the core layer of cast stretch film. It provides excellent clarity and ultimate stretch values higher than the more conventional 2.0-2.5 MI cas.. |
|||
Secant Modulus, MD | 0.152 GPa | 22.0 ksi | ASTM D882 |
Huntsman PE1353 EVA Film Extrusion