Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 27.6 - 34.5 MPa | 4000 - 5000 psi | ASTM D732 |
Mar-Bal MB2000-5 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Shear Strength | 27.6 - 34.5 MPa | 4000 - 5000 psi | ASTM D732 |
Mar-Bal MB2000-8 Thermoset Polyester Composite Molding Compound An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can.. |
|||
Shear Strength | 17.2 - 34.5 MPa | 2500 - 5000 psi | Lap; ASTM D1002 |
3M Scotch-Weld™ RT38 Retaining Compound Anaerobic Adhesives 3M™ Scotch-Weld™ Retaining Compound Anaerobic Adhesives are one-component anaerobic adhesives designed to secure cylindrical metal assemblies such as bearings on shafts, bushing, sleeves, housings.. |