Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 5.00 - 10.0 MPa | 725 - 1450 psi | Cured; ASTM D1002/DIN 53283 |
Palm Labs Adhesives Turbo Fuse Series 130PR PLASTIC & RUBBER (100 Viscosity) Rapid Bonding Adhesive Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE SERIES 130PR PLASTIC & RUBBER’S advanced formula is designed to polymerize instantly by absorbing surface moisture. Th.. |
|||
Shear Strength | 3.00 - 10.0 MPa | 435 - 1450 psi | ISO 10123; Compressive, Steel pins and collars |
Palm Labs Adhesives TURBO-LOCK SERIES 10 Anaerobic Thread Locking Compound TURBO-LOCK SERIES 10 is a removable, PURPLE, fast curing, low strength, anaerobic thread-locking compound for bonding and sealing small screw threads. It is highly resistance to heat, vibrations, wa.. |
|||
Shear Strength | 5.00 - 10.0 MPa | 725 - 1450 psi | polycarbonate; ASTM D1002/DIN 53283 |
BCC Products BC 100 Thin Cyanoacrylate Adhesive BC100 Thin is a low viscosity material ideal for bonding larger areas. BC100 Thin has a 20 second fixture cure and able to fill gaps of .002” wide. BC100 Thin is perfectly designed for bonding plas.. |
|||
Shear Strength | 5.00 - 10.0 MPa | 725 - 1450 psi | polycarbonate; ASTM D1002/DIN 53283 |
BCC Products BC 100 Thick Cyanoacrylate Adhesive BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to f.. |